                    [Title] => DOST-FPRDI develops wood ‘super dryer’
                    [Summary] => Now, a 50-millimeter thick lumber can be dried in just 24 days instead of the maximum 198 days and just 10 days to kiln-dry a 25-mm thick gmelina wood instead of 75-150 days.


This is possible with the use of the furnace-type lumber dryer developed by the Los Baños-based Department of Science and Technology-Forest Products Research and Development Institute (DOST-FPRDI).

In drying experiments done by the institution, it was found that the seasoning time for the hard-to-dry gmelina can be cut by as much as 93 percent.
[DatePublished] => 2001-10-22 00:00:00 [ColumnID] => 133272 [Focus] => 0 [AuthorID] => [AuthorName] => [SectionName] => Real Estate [SectionUrl] => real-estate [URL] => ) [1] => Array ( [ArticleID] => 136603 [Title] => Fast drying method for wood developed [Summary] => It is now possible to kiln-dry a 25-millimeter thick gmelina wood in 10 days instead of the usual 75-150 days. Likewise, one can now dry a 50-mm lumber in 24 days instead of 119 to 198 days.

The seasoning time for the hard-to-dry gmelina (scientific name: Gmelina arborea) has been considerably shortened by a furnace-type lumber dryer developed by the Los Baños-based Forest Products Research and Development Institute (FPRDI), an agency under the Department of Science and Technology (DOST).
[DatePublished] => 2001-10-14 00:00:00 [ColumnID] => 133272 [Focus] => 0 [AuthorID] => [AuthorName] => [SectionName] => Agriculture [SectionUrl] => agriculture [URL] => ) ) )
NORTHLANDIA ENTERPRISE
Array
(
    [results] => Array
        (
            [0] => Array
                (
                    [ArticleID] => 137501
                    [Title] => DOST-FPRDI develops wood ‘super dryer’
                    [Summary] => Now, a 50-millimeter thick lumber can be dried in just 24 days instead of the maximum 198 days and just 10 days to kiln-dry a 25-mm thick gmelina wood instead of 75-150 days.


This is possible with the use of the furnace-type lumber dryer developed by the Los Baños-based Department of Science and Technology-Forest Products Research and Development Institute (DOST-FPRDI).

In drying experiments done by the institution, it was found that the seasoning time for the hard-to-dry gmelina can be cut by as much as 93 percent.
[DatePublished] => 2001-10-22 00:00:00 [ColumnID] => 133272 [Focus] => 0 [AuthorID] => [AuthorName] => [SectionName] => Real Estate [SectionUrl] => real-estate [URL] => ) [1] => Array ( [ArticleID] => 136603 [Title] => Fast drying method for wood developed [Summary] => It is now possible to kiln-dry a 25-millimeter thick gmelina wood in 10 days instead of the usual 75-150 days. Likewise, one can now dry a 50-mm lumber in 24 days instead of 119 to 198 days.

The seasoning time for the hard-to-dry gmelina (scientific name: Gmelina arborea) has been considerably shortened by a furnace-type lumber dryer developed by the Los Baños-based Forest Products Research and Development Institute (FPRDI), an agency under the Department of Science and Technology (DOST).
[DatePublished] => 2001-10-14 00:00:00 [ColumnID] => 133272 [Focus] => 0 [AuthorID] => [AuthorName] => [SectionName] => Agriculture [SectionUrl] => agriculture [URL] => ) ) )
abtest
Are you sure you want to log out?
X
Login

Philstar.com is one of the most vibrant, opinionated, discerning communities of readers on cyberspace. With your meaningful insights, help shape the stories that can shape the country. Sign up now!

Get Updated:

Signup for the News Round now

FORGOT PASSWORD?
SIGN IN
or sign in with